This publication presents an overview of a decade-long series of programs which exposed welded coupon and full diameter pipe in chlorination and chlorine dioxide bleaching equipment. Findings have guided procedures for the fabrication and post fabrication clean-up of over 75 6% Mo stainless steel wa...

Descripción completa

Detalles Bibliográficos
Clasificación:Libro Electrónico
Autores principales: Tuthill, Arthur H. (Autor), Avery, Richard E. (Autor), Garner, Andrew (Autor)
Formato: Electrónico eBook
Idioma:Inglés
Publicado: Toronto, Ont. : Nickel Development Institute, 1992.
Colección:Technical series (Nickel Development Institute (Canada)) ; no. 14 026.
Temas:
Acceso en línea:Texto completo

MARC

LEADER 00000cam a2200000 i 4500
001 KNOVEL_on1255595075
003 OCoLC
005 20231027140348.0
006 m o d
007 cr |||||||||||
008 210609s1992 onca ob 000 0 eng d
040 |a HUA  |b eng  |e rda  |e pn  |c HUA  |d HUA  |d OCLCO  |d OCLCF  |d OCLCO  |d UAB 
020 |a 9781523131075  |q (electronic bk.) 
020 |a 1523131071  |q (electronic bk.) 
029 1 |a AU@  |b 000071347526 
029 1 |a AU@  |b 000068006222 
035 |a (OCoLC)1255595075 
050 4 |a Internet Access  |b AEU 
082 0 4 |a 620.1623  |2 23 
049 |a UAMI 
100 1 |a Tuthill, Arthur H.,  |e author. 
245 1 0 |a Corrosion behaviour of stainless steel, nickel base alloy and titanium weldments in chlorination and chlorine dioxide bleaching /  |c Arthur H. Tuthill, Richard E. Avery, and Andrew Garner. 
264 1 |a Toronto, Ont. :  |b Nickel Development Institute,  |c 1992. 
300 |a 1 online resource (20 pages) :  |b illustrations 
336 |a text  |b txt  |2 rdacontent 
337 |a computer  |b c  |2 rdamedia 
338 |a online resource  |b cr  |2 rdacarrier 
490 1 |a NiDI reprint series ;  |v no. 14 026 
500 |a "Reprinted with permission from Proceedings of the Technical Association of the Pulp and Paper Industry, TAPPI, 7th International Symposium on Corrosion in the Pulp and Paper Industry, Orlando, FL, 1992" 
504 |a Includes bibliographical references. 
520 |a This publication presents an overview of a decade-long series of programs which exposed welded coupon and full diameter pipe in chlorination and chlorine dioxide bleaching equipment. Findings have guided procedures for the fabrication and post fabrication clean-up of over 75 6% Mo stainless steel washers. Findings are also applicable to 6% Mo, nickel base alloy, clad nickel base alloy, titanium and plastic-lined piping for bleach plants. Guidelines for procurement and fabrication of piping materials are included. Applicability to mixer-to-tower, tower-to-vat and filtrate piping sections is reported. 
590 |a Knovel  |b ACADEMIC - Welding Engineering & Materials Joining 
590 |a Knovel  |b ACADEMIC - Metals & Metallurgy 
650 0 |a Alloys  |x Corrosion. 
650 0 |a Bleaching industry  |x Equipment and supplies  |x Corrosion. 
650 6 |a Alliages  |x Corrosion. 
650 7 |a Alloys  |x Corrosion.  |2 fast  |0 (OCoLC)fst00805710 
700 1 |a Avery, Richard E.,  |e author. 
700 1 |a Garner, Andrew,  |e author. 
776 0 8 |i Print version:  |a Tuthill, Arthur H.  |t Corrosion behaviour of stainless steel, nickel base alloy and titanium weldments in chlorination and chlorine dioxide bleaching 
830 0 |a Technical series (Nickel Development Institute (Canada)) ;  |v no. 14 026. 
856 4 0 |u https://appknovel.uam.elogim.com/kn/resources/kpCBSSNBAB/toc  |z Texto completo 
994 |a 92  |b IZTAP